Wire and cable insulation accounts for a major share of global flexible PVC consumption. As electrical infrastructure, automotive harnesses, renewable energy cabling and appliance cords face stricter environmental and thermal standards, cable compounders are reformulating away from restricted ortho-phthalates toward low-volatility, RoHS-compliant plasticizer systems. Selecting the right plasticizer package directly determines whether a cable compound passes heat-aging retention, volume resistivity and cold-bend tests.
Unlike general film or profile extrusion, PVC wire and cable jacketing subjects the plasticizer to continuous thermal load during service and high shear during high-speed extrusion. Four indicators govern plasticizer selection in cable compounds:
Low Volatility and Heat-Aging Retention: High mass loss during oven aging leads to brittle insulation and failed elongation-at-break tests.
Volume Resistivity (Electrical Insulation): Ionic impurities, high acid value or excessive moisture sharply degrade electrical insulation resistance.
Low-Temperature Flexibility: Outdoor and cold-climate cables must pass cold-bend and cold-impact testing without cracking.
RoHS (EU) 2015/863 Compliance: Export-oriented cable harnesses must remain below the 0.1% limit for DEHP, BBP, DBP and DIBP.
Different cable temperature classes (70 °C, 90 °C, 105 °C and cold-resistant grades) require distinct plasticizer backbones or synergistic blends. The table below outlines how DOBO's core cable plasticizer grades compare in formulation design.
Plasticizer Grade | CAS No. / Series | Primary Advantage in Cable PVC | Typical Cable Application |
DOTP (Dioctyl Terephthalate) | CAS 6422-86-2 | Higher volume resistivity and lower volatility than DOP; 100% phthalate-free | 70 °C – 90 °C building wire, appliance cords, flexible sheathing |
Cable-Grade DINCH | CAS 166412-78-8 | Low migration, strong cold flexibility and halogen-free/phthalate-free compliance | Medical equipment cables, indoor communication cables, low-odor harnesses |
TOTM (Trioctyl Trimellitate) | CAS 3319-31-1 | Ultra-low volatility, high flash point and superior thermal aging stability | 105 °C heat-resistant insulation, automotive under-hood wiring |
DOS / DOA (Aliphatic Esters) | CAS 122-62-3 / 103-23-1 | Exceptional low-temperature plasticizing efficiency down to −40 °C to −60 °C | Secondary cold-resistant plasticizer blended with DOTP or TOTM for outdoor cables |
Cable Exclusive Plasticizer DB44 | DOBO DB44 Series | Formulated for balanced dry-blend uptake, electrical insulation and extrusion output | General PVC cable jacketing and insulation compounds |
When replacing DOP in 70 °C and 90 °C PVC cable compounds, DOTP (CAS 6422-86-2) delivers two immediate technical advantages in addition to phthalate-free compliance:
Higher Volume Resistivity: Because of its symmetrical para-substituted structure and lower polarity, DOTP reduces ionic mobility in the PVC matrix, resulting in higher volume resistivity than DOP at equivalent PHR loadings.
Lower Volatility in Oven Aging: DOTP has a higher flash point (approx. 238 °C) and lower vapor pressure than DOP, helping cable jacketing retain tensile strength and elongation after 100 °C × 168 h heat-aging tests.
Even minor batch-to-batch fluctuations in a plasticizer can cause die drool, porosity or dielectric breakdown on a high-speed cable extrusion line. Buyers should verify the following parameters on every batch COA:
Acid Value (≤0.1 mg KOH/g): Elevated acidity indicates residual catalyst or hydrolysis, which lowers volume resistivity.
Water Content (≤0.1%): Excess moisture causes micro-voids during high-temperature extrusion and reduces dielectric breakdown voltage.
Color (Pt-Co ≤25): Ensures clean color matching for color-coded phase insulation wires.
Flash Point: Confirms absence of light-end volatile contamination.
Cable Grade DINCH Plasticizer CAS 166412-78-8 - Wire & Cable PVC Plasticizer
Dioctyl Terephthalate DOTP Plasticizer CAS 6422-86-2 (99% Purity)
Yes. Blending DOTP with TOTM is widely used by cable compounders to achieve 90 °C and 105 °C thermal aging requirements while optimizing dry-blend absorption and overall formulation economics.
Replacing 10–20% of the primary DOTP dosage with an aliphatic diester such as DOS (dioctyl sebacate) or DOA (dioctyl adipate) significantly lowers the brittle temperature while maintaining good compatibility.
DOBO supplies liquid plasticizers in 200 kg galvanized drums, 1000 kg IBC totes and flexitanks for full-container shipments from Ningbo, China, accompanied by batch COA and SDS documentation.
Transitioning PVC wire and cable compounds to eco-friendly plasticizers requires matching the ester backbone to the target thermal class and electrical specification. Whether your line runs DOTP for general sheathing, DINCH for halogen-free indoor cables, TOTM for 105 °C insulation, or DOBO's Cable Exclusive Plasticizer DB44, consistent low acid value and low moisture are essential. Contact NINGBO DONGBO NEW ENERGY CO., LTD. (DOBO) to request technical data sheets and trial samples.