| Quantity: | |
|---|---|
TOTM-99
DOBO
TOTM-DB01
TOTM (trioctyl trimellitate, CAS 3319-31-1), also written as tris(2-ethylhexyl) trimellitate, is a high-molecular-weight trimellitate ester used where conventional plasticizers evaporate too quickly. It is the reference grade for 105 °C cable compounds, automotive interior and under-bonnet parts, gaskets, sealing profiles and appliance wiring, because it combines low volatility with strong resistance to extraction and migration. NINGBO DONGBO NEW ENERGY CO., LTD. (DOBO) supplies TOTM as a clear, low-colour liquid for PVC and polymer processing.
The table below summarises the typical property profile of TOTM. Values are for general reference during grade selection and are not a purchase specification; lot-specific data is issued on the certificate of analysis.
| Property | Typical Value | Remark |
| Chemical name | Trioctyl trimellitate (tris(2-ethylhexyl) trimellitate) | Trimellitate ester |
| CAS number | 3319-31-1 | EINECS 222-020-0 |
| Molecular formula | C33H54O6 | MW 546.87 |
| Appearance | Clear, colourless to pale yellow oily liquid | Visual |
| Ester content | ≥ 98.0 % | Min. |
| Colour | ≤ 30 APHA | Platinum-cobalt |
| Acid value | ≤ 0.10 mg KOH/g | After heating also ≤ 0.10 |
| Heating loss | ≤ 0.10 % | Low volatility indicator |
| Density (20/20 °C) | 0.990 ± 0.003 g/cm3 | — |
| Refractive index (nD25) | 1.485 ± 0.003 | Identity check |
| Freezing point | < −50 °C | Cold-end performance |
| Flash point | ≈ 254 °C | High flash, low fire risk in storage |
| Volume resistivity | ≥ 5.0 × 1011 Ω·cm | Electrical grade suitability |
In a 105 °C rated cable, the plasticizer has to survive years of conductor heat without evaporating out of the insulation. TOTM's molecular weight of about 547 g/mol is roughly double that of DOP, so its diffusion rate through the PVC matrix is far lower. The practical consequences are visible in three routine tests:
TOTM is specified for heat-resistant PVC insulation, appliance wiring, automotive cable and industrial control cable. Because volume resistivity remains above 5 × 1011 Ω·cm, it is also used in compounds where electrical performance cannot be traded for heat resistance. Typical loadings sit in the same range as DINP or DOTP for a given hardness, so existing extrusion lines usually need only a minor temperature-profile adjustment because TOTM gels more slowly.
Fogging, hardening and plasticizer migration onto painted trim are the classic automotive complaints. TOTM's low volatility makes it a common base for instrument-panel skins, cable jacketing, grommets and under-bonnet sleeves, either alone or blended with DINCH or DOTP to balance cost and cold flexibility.
Sealing profiles need to stay soft for decades while being squeezed against a frame. Low migration means the gasket does not stain the surrounding surface and does not shrink away from the profile groove. TOTM is frequently used in refrigerator gaskets, construction seals and industrial O-ring compounds where permanent softness matters more than initial cost.
Engine hoses, heat-shielded sleeves and industrial sheet benefit from the same characteristics: minimal weight loss in hot air, retained elongation, and no oily film on the surface after storage. In these applications TOTM is often combined with a polymeric plasticizer when extreme oil contact is also expected.
TOTM is not an ortho-phthalate and is therefore outside the phthalate restrictions that drive the move away from DOP and DINP in toys, childcare articles and food-contact applications. For each lot DOBO can provide a certificate of analysis covering ester content, colour, acid value, heating loss, density and water content, together with a safety data sheet. Buyers should confirm the applicable regulation for their own market and end use before finalising a specification.
TOTM is supplied in steel drums and intermediate bulk containers; the packing configuration is confirmed with the order. Drums should be stored upright, sealed and protected from water ingress. Shelf life under proper storage is normally stated on the certificate and is typically two years from production.
No. TOTM is a trimellitate ester of 2-ethylhexanol, not an ortho-phthalate, and is therefore not covered by the ortho-phthalate restrictions applied to DOP, DBP, BBP and DEHP.
Usually yes at similar phr, but expect slower gelation and a slightly different hardness response. Run a short trial at the same Shore A target and check elongation and cold bend before switching a full order.
DOTP performs well in general-purpose and 70 °C to 90 °C compounds. Above that, TOTM's higher molecular weight and lower volatility give better retention of elongation and hardness after long-term heat ageing.
Volume resistivity of the neat ester is typically at or above 5 × 1011 Ω·cm, which is why trimellitates are used in insulation compounds. Final compound resistivity still depends on filler, stabilizer and contamination control.
DOBO supplies TOTM and the full range of general-purpose and application-specific plasticizers, including DOTP, DINP, DOP, DOA, DOS, DINCH and the DB11 to DB99 series. Contact our technical team with your hardness target, processing route and temperature class, and we will confirm the grade and documentation you need. For a broader comparison of heat-resistant options, read our article on TOTM versus traditional PVC plasticizers.